Aluminum resists corrosion because a thin natural oxide film forms on its surface and separates the metal from its surroundings. Aluminum corrosion happens when that film is broken down, either locally by chlorides, trapped moisture or contact with another metal, or chemically by strong acids and alkalis.

  • Pitting and crevice
  • Galvanic
  • Intergranular and filiform

Why aluminum resists corrosion: the oxide film

Bare aluminum exposed to air forms a thin oxide film. The film is tightly bonded to the metal and it keeps water and oxygen from reaching the metal underneath. If the surface is scratched in air, a new film forms over the damage, so in ordinary conditions the protection repairs itself.

The film is stable in near-neutral conditions, which covers most rain, fresh water and indoor air. Strong acids and strong alkalis dissolve it, and the metal then corrodes in a way the film would otherwise prevent. Wet cement and mortar are alkaline, as are some cleaning agents, which is why fresh masonry and harsh cleaners are kept off aluminum surfaces.

Corrosion of aluminum in service is typically local: something breaks the film at one spot and stops it from reforming. The types below differ in what does the breaking.

Types of aluminum corrosion

Pitting

Pitting is local attack that forms small cavities while the surrounding surface stays sound. Chlorides, for example sea salt and de-icing salt, are a common cause of pitting on aluminum: they break the oxide film at weak points, and the small exposed area corrodes. On bare aluminum, pits are often covered by a white, powdery corrosion product. Pitting is worse where salt deposits stay damp and are not rinsed off by rain.

Crevice corrosion

Crevice corrosion starts in narrow gaps where water can get in but cannot drain or dry out: laps between sheets, the space under a washer or gasket, or under dirt and debris. Inside the gap the trapped water loses oxygen and becomes more aggressive, so the oxide film breaks down and the metal corrodes, often out of sight.

Galvanic corrosion

Galvanic corrosion happens when two different metals are in electrical contact and wetted by the same electrolyte, such as rainwater carrying salt. The more active metal then corrodes faster than it would alone, and the more noble metal corrodes less.

ASTM G82 describes how a galvanic series is built: metals are ranked by the corrosion potentials observed in a specific environment, and the series applies to that environment. The standard notes that a larger difference in potential frequently, though not always, means more galvanic corrosion.

Published seawater galvanic series place aluminum alloys toward the active end, close to zinc. Steel, stainless steel and copper all sit on the more noble side, so contact with any of them can accelerate corrosion of the aluminum. The effect is generally larger with copper alloys and stainless steel than with carbon steel. The rate also depends on how conductive the water is and on the relative areas of the two metals, so avoid a small area of aluminum against a large area of a more noble metal.

Intergranular corrosion in 5xxx alloys

Intergranular corrosion follows the grain boundaries instead of spreading across the surface. In some 5xxx (aluminum-magnesium) alloys, depending on composition and thermal history, an aluminum-magnesium compound can precipitate along the grain boundaries. When it forms a fairly continuous network, the boundaries corrode preferentially. This is mainly a concern for higher-magnesium 5xxx alloys exposed to raised temperatures over long periods.

ASTM G67, the nitric acid mass loss test (NAMLT), measures this susceptibility in 5xxx alloys. Samples are kept immersed in nitric acid, which preferentially dissolves the compound where it lies along the grain boundaries, and the mass lost indicates how susceptible the material is. Where this matters, ask whether G67 results apply to the alloy and temper offered.

Filiform corrosion

Filiform corrosion is specific to coated metal: thin threads of corrosion grow under the paint film, starting from a cut edge, scratch or coating defect, and show as raised, wandering lines in the finish. The filiform corrosion guide for coated aluminum covers causes, testing and prevention.

How design, coatings and alloy choice prevent each type

Each type has a different cause, so prevention works at a different point. This is general guidance; the right detail depends on the exposure.

Corrosion types on aluminum: cause and prevention
TypeCausePrevention in designCoating or alloy
Chemical attackStrong acids or alkalis dissolve the oxide filmKeep wet mortar, cement and harsh cleaners off the metalAn intact coating keeps the chemical off the surface
PittingChlorides break the film locallyDrain surfaces, avoid standing water, wash sheltered areasIntact coating with protected cut edges; alloys with copper as a main alloying element (2xxx) are generally less resistant than 1xxx, 3xxx and 5xxx
CreviceStagnant water trapped in narrow gapsSeal gaps or open them so they drain and dry; store sheet dry. Water trapped between wet sheets or coil wraps can stain the surface; see the guide to receiving, storing and handling coated coil.Coat parts before assembly; seal laps
GalvanicContact with a more noble metal plus an electrolyteIsolate dissimilar metals, choose compatible fasteners, route copper runoff awayCoat the more noble metal, or both
IntergranularGrain-boundary precipitation in susceptible 5xxx alloysMatch alloy and temper to the service conditionsSpecify the alloy and temper; ask whether ASTM G67 results apply
FiliformCorrosion spreading under paint from a defect or cut edgeProtect cut edges, avoid coating damage, keep coil dryPretreatment, matched primer and topcoat, edge treatment

Preventing galvanic corrosion between aluminum and steel

A galvanic cell needs three things: two different metals, electrical contact between them, and an electrolyte bridging them. Remove any one and the cell stops, whether the other metal is steel, stainless steel or copper.

  • Isolate dissimilar metals. Put a nonconductive separator, such as a plastic or rubber washer, a tape or a gasket, between the aluminum and the other metal, and detail the joint so it does not hold water.
  • Choose compatible fasteners. Aluminum fasteners avoid the dissimilar pair altogether. Where stainless steel fasteners are used, isolate them with washers, and keep the fastener small relative to the aluminum it holds rather than the reverse.
  • Avoid copper runoff onto aluminum. Rainwater running off copper onto aluminum is a known galvanic risk. Route that drainage away from aluminum surfaces.
  • Coat the more noble side. If only one metal can be coated, coat the more noble one, or both; coating only the aluminum can concentrate attack at any defect.

Coastal exposure: coating, cut edges and washing

Salt-laden air near the sea raises the risk of pitting, crevice, galvanic and filiform corrosion at once, so coastal projects depend more on the coating system and detailing.

Choose the coating system for the exposure

Coating systems differ in how they hold up to salt, UV and moisture. For aggressive exposure, compare systems on the supplier's evidence for that environment, not on the system name alone. The PVDF coated aluminum page covers one system used for exterior work. Orbit supplies prepainted aluminum coil in 1xxx, 3xxx and 5xxx alloys, with 3105 as the main coated substrate, in PE, HDPE, PVDF, PU, PUPA, Epoxy, Acrylic and Epoxy-PE systems. Coating warranties run 5 to 20 years depending on application and environment, with terms confirmed per order, so state the exposure in the request.

Protect cut edges

Slitting, shearing and punching leave bare aluminum at the cut edge. On coated sheet, edges are a typical starting point for pitting and filiform corrosion. Detail cut edges so they drain and do not sit in water, and where the specification calls for it, seal or touch up edges with a product compatible with the coating.

Wash what the rain does not reach

Rain rinses salt off exposed surfaces, but sheltered areas such as soffits, the undersides of overhangs and recessed panels collect salt and stay damp. Periodic washing of those areas with clean water and a mild, neutral cleaner removes deposits before they build up.

Standards referenced

  • ASTM G82, guide to building and using a galvanic series for predicting galvanic corrosion
  • ASTM G67, nitric acid mass loss test (NAMLT) for intergranular corrosion susceptibility of 5xxx alloys

Corrosion questions.

Does aluminum rust?

No. Rust is iron oxide and forms on iron and steel. Aluminum forms its own thin oxide film, which protects it in near-neutral conditions. Where aluminum does corrode, the product is typically a white, powdery deposit rather than red rust.

What causes aluminum to corrode?

Breakdown of the natural oxide film. It can be broken locally by chlorides, by stagnant moisture in crevices or by contact with a more noble metal, or chemically by strong acids and alkalis.

Can aluminum be in contact with steel?

It can, if the joint is designed for it. Contact with steel in the presence of water can cause galvanic corrosion of the aluminum. Isolate the two metals with a nonconductive separator, keep the joint dry and coat the steel or both metals.

Are stainless steel fasteners safe in aluminum?

Stainless steel is more noble than aluminum, so in wet, salty conditions the aluminum around the fastener can corrode. Isolating washers and a small fastener area relative to the aluminum reduce the risk.

What is ASTM G67 used for?

ASTM G67 measures the susceptibility of 5xxx alloys to intergranular corrosion, using constant immersion in nitric acid and measuring the mass lost.

Does a coating stop aluminum corrosion?

An intact, well-bonded coating greatly slows water, salt and chemicals reaching the metal. The protection depends on the coating staying intact, so cut edges, scratches and fastener holes need attention.

Specifying coil for a corrosive site?

Send the alloy, coating system, exposure, thickness, width, quantity and destination. We respond to RFQs within one business day.

Request a Quote