Reference · Standards
ASTM B209: the aluminum sheet and plate standard explained.
ASTM B209 is the ASTM specification for aluminum and aluminum-alloy sheet and plate. It sets the requirements a mill product has to meet, alloy by alloy and temper by temper, and gives buyer and producer one reference for acceptance. This page explains what ASTM B209 covers, how it shows up on a certificate and how it compares with EN 485.
- Sheet, coiled sheet and plate
- Alloys and tempers in its tables
- US tolerances: ANSI H35.2
What is ASTM B209?
The full title is "Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate". It is published as ASTM B209/B209M: one document with inch-pound (B209) and SI (B209M) values. Each set of values is used on its own, and the two are not combined. Like every ASTM standard, it is revised from time to time, and each edition carries a year suffix. At the time of writing (November 2026) the active edition is B209/B209M-21a.
B209 is a product specification. It does not tell a mill how to roll metal. It tells the buyer and the producer what the delivered sheet or plate has to be, and gives both sides a shared reference for acceptance. When a purchase order says "ASTM B209, 3003-H14", the standard and that designation fix the alloy and temper requirements, though thickness, width, finish and other order details must still be stated.
What does ASTM B209 aluminum sheet cover?
The scope covers aluminum and aluminum-alloy flat sheet, coiled sheet and plate, in the alloys and tempers listed in the tables of the standard. An alloy and temper combination that is not in those tables is outside B209, even if a mill can make it. The scope itself does not state a thickness range, so check the tables of the standard for the alloy, temper and product you are ordering rather than assuming a limit.
The finishes B209 recognizes are:
- Mill finish, the surface as it comes off the rolling mill, for all products in the scope.
- One-side bright, standard one-side bright and standard two-sides bright, which apply to non-heat-treatable sheet only.
Tread plate, the raised-pattern plate used for flooring and steps, is not covered by B209. It has its own specification, ASTM B632/B632M. Painted finishes are not a B209 finish either: when sheet is coil coated, B209 still describes the aluminum underneath, and the paint system has its own specification. Architectural coating performance is covered separately by FGIA's AAMA 2603, 2604 and 2605 specifications.
What B209 specifies
The numbers themselves are in the standard and are not reproduced here. Among its main requirements, the standard ties these to each alloy and temper:
| Requirement | What it controls | Where the values come from |
|---|---|---|
| Chemical composition | The alloy has to fall inside the composition limits for its alloy designation | B209 uses ANSI H35.1 alloy and temper designations; composition limits follow the Aluminum Association registrations |
| Mechanical properties | Tensile strength, yield strength and elongation for each alloy and temper | B209 sets mechanical property requirements by alloy and temper |
| Dimensional tolerances | Permitted dimensional variation | ANSI H35.2, dimensional tolerances for US sheet and plate (and other mill products) |
| Finish | The surface condition supplied | The finishes listed in the scope, as above |
The practical point for a buyer is that "ASTM B209" alone is not a complete order. The standard only becomes specific when the alloy, temper, thickness and finish are stated next to it, because those choose the row of each table that applies.
Is there an ASTM B209 PDF?
ASTM sells B209 as a PDF or in print on its store; it is a copyrighted document. A copy found elsewhere may be unauthorized or an old edition, and an old edition can differ from the one your contract names. If your order or a customer specification cites B209, buy the current edition from ASTM, or confirm which edition the contract calls for and buy that one.
This page does not host or link copies of ASTM standards; buy them from ASTM.
How B209 appears on a mill test report
A mill test report, or material certificate, shows the material against a named specification. For B209 material you would usually find the standard designation (often with its edition year), the alloy and temper, the measured chemical composition, the results of mechanical tests on samples from the lot, the dimensions and a lot or batch number that ties the paper to the coil. The reported results are compared with the limits for that alloy and temper in the standard.
Two checks are worth doing every time: that the standard on the certificate is the one on your purchase order, and that the alloy and temper match the order. For a line-by-line walk through a certificate, see our guide to reading a mill test report for aluminum coil.
B209 vs EN 485
In Europe, and in other markets that work to EN standards, flat-rolled aluminum is ordered to EN 485 instead. EN 485 splits the job into parts, and refers to separate standards for composition and tempers. B209 keeps most of it in one specification; US dimensional tolerances are set in ANSI H35.2.
| Requirement | EN system | ASTM system |
|---|---|---|
| Inspection and delivery | EN 485-1, technical conditions for inspection and delivery | Within B209 |
| Mechanical properties | EN 485-2, mechanical properties | B209 mechanical property requirements by alloy and temper |
| Tolerances, hot-rolled | EN 485-3, tolerances on dimensions and form for hot-rolled products | ANSI H35.2 |
| Tolerances, cold-rolled | EN 485-4, tolerances on shape and dimensions for cold-rolled products, over 0.20 up to 50 mm | ANSI H35.2 |
| Chemical composition | EN 573-3 | Composition limits follow the Aluminum Association registrations |
| Temper designations | EN 515 | ANSI H35.1 designations (used by B209); tempers listed in the B209 tables |
The two systems were written separately and are not interchangeable. A certificate is issued against the standard named on the order, so pick one, name it with its edition where you can, and do not assume a part that meets one system has been tested to the other.
Ordering sheet to ASTM or EN from Orbit
Orbit supplies to ASTM or EN standards depending on the market, with material certificates with every batch. Tell us on the RFQ which standard governs your order. The relevant facts for flat-rolled orders:
- Integrated aluminum coil manufacturer in Aqaba, Jordan, family owned and operating since 1976.
- Metal melted and cast by Orbit in Jordan. Certificate of origin available.
- Rolled aluminum coil from 0.20 to 2.00 mm thick, up to 1650 mm wide, coil weight up to 10 tonnes.
- Alloys in the 1xxx, 3xxx and 5xxx series.
- Slitting, cut-to-length, embossing and coil coating capabilities.
- ISO 9001, ISO 14001 and ISO 45001 certified.
- MOQ 6.5 MT.
Standards referenced
- ASTM B209/B209M, Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate
- ASTM B632/B632M, specification for aluminum tread plate
- ANSI H35.1, alloy and temper designation systems for aluminum
- ANSI H35.2, dimensional tolerances for aluminum mill products
- EN 485-1, technical conditions for inspection and delivery
- EN 485-2, mechanical properties
- EN 485-3, tolerances on dimensions and form for hot-rolled products
- EN 485-4, tolerances on shape and dimensions for cold-rolled products
- EN 573-3, chemical composition
- EN 515, temper designations
- FGIA AAMA 2603, 2604 and 2605, architectural coating specifications
ASTM B209 questions.
What does ASTM B209 cover?
ASTM B209 is the specification for aluminum and aluminum-alloy flat sheet, coiled sheet and plate, in the alloys and tempers listed in its tables. It sets requirements for composition, mechanical properties and finish. Dimensional tolerances for US aluminum sheet and plate are set in ANSI H35.2.
Where can I get the ASTM B209 PDF?
ASTM International sells ASTM B209 on the ASTM store as a PDF or in print. The standard is copyrighted; this page does not host or link copies of ASTM standards, so buy them from ASTM.
What is the difference between B209 and B209M?
They are one document, ASTM B209/B209M, with inch-pound (B209) and SI (B209M) values. Each set of values is used on its own, and the two are not combined.
Does ASTM B209 cover tread plate?
No. Tread plate is covered by its own specification, ASTM B632/B632M.
Does ASTM B209 cover painted aluminum sheet?
B209 covers the aluminum sheet itself, with mill finish and, for non-heat-treatable sheet, bright finishes. A paint or coil coating system is specified separately, so a painted sheet order usually names B209 for the metal and a coating specification for the paint.
Is ASTM B209 the same as EN 485?
No. Both cover flat-rolled aluminum, but they are separate systems. EN 485 is split into four parts and refers to EN 573-3 for composition and EN 515 for tempers, while B209 keeps most requirements in one document. US dimensional tolerances are set in ANSI H35.2. Name one standard on the order.
Does Orbit supply to ASTM B209?
Orbit supplies to ASTM or EN standards depending on the market, with material certificates with every batch. State the standard your order needs on the RFQ.
Ordering sheet or coil to a standard?
Send the standard, alloy, temper, thickness, width, finish, quantity and destination. We respond to RFQs within one business day.