Reference · Corrosion
Filiform corrosion on coated aluminum: causes and prevention.
Filiform corrosion is thread-like corrosion that spreads under a coating from a defect, a scratch or a cut edge. On coated aluminum it shows as fine, wandering lines under the paint, and it is prevented mainly through pretreatment, the coating system and care of cut edges in fabrication.
- Starts at edges and defects
- Test: EN ISO 4623-2
- Pretreatment and edge care
What is filiform corrosion?
Filiform corrosion is a form of corrosion that runs under a coating. It begins where the coating is broken, at a cut edge, a scratch, a pinhole or a fastener hole, and spreads beneath the intact paint as thin threads.
The paint over each thread lifts slightly, so the threads show as raised lines that wander across the surface. Each thread has an active head that advances and a tail behind it filled with corrosion product. Threads can branch, and several often start from the same edge or scratch.
It is mainly an appearance and adhesion problem. The finish is disfigured, and the coating along each thread is loosened from the metal, so threads left to grow can end in flaking paint. For pitting, crevice, galvanic and intergranular attack on aluminum, see the guide to aluminum corrosion types.
Why it starts at cut edges, scratches and coating defects
Filiform corrosion needs a way in. Where the coating is continuous and well bonded, far less moisture and salt reaches the metal surface. A break in the film changes that:
- A cut edge from slitting, shearing or punching exposes bare aluminum and the boundary between metal, pretreatment and paint.
- A scratch or impact does the same in the middle of a panel.
- A pinhole, crater or poorly cured area leaves a weak spot in a film that otherwise looks sound.
Once corrosion begins at one of these points, it can travel along the interface between the metal and the coating. That is why the bond at the interface matters, not only the paint film on top of it.
The role of moisture and chlorides
Filiform corrosion develops in humid conditions, and it is generally started by a contaminant at the defect, such as chloride. Coastal air, de-icing salt and some industrial atmospheres supply chlorides, and warm, humid conditions keep the defect moist enough for the threads to grow.
Where a surface sits also matters. Sheltered areas that rain does not rinse collect salt and stay damp for longer, so they are more exposed than surfaces that are washed by rain and dry quickly. The same applies to coil and sheet in storage: a damp, salty warehouse air works on cut edges before the material is ever installed.
What pretreatment does
Pretreatment is the chemical layer applied to cleaned aluminum before the primer on a coil coating line. Its job is to give the primer a well-bonded surface and to slow corrosion at the metal-coating interface. Because filiform corrosion travels along the boundary between metal and coating, the cleaning and pretreatment stages have a direct bearing on how far threads can spread once they start.
The pretreatment and primer stages of the coil coating process are explained step by step in a separate post. For a specification, ask the coater to state the pretreatment applied and the evidence that supports it for your exposure.
How filiform resistance is tested
EN ISO 4623-2, Paints and varnishes, Determination of resistance to filiform corrosion, Part 2: Aluminium substrates, is the laboratory test written for coated aluminum. Coated panels are scribed through the coating to the metal, exposed to conditions that start and promote filiform corrosion, and then examined for the thread-like corrosion spreading from the scribe.
A result is a comparison of coatings under set laboratory conditions, not a service-life figure for a particular climate. If filiform resistance matters to a project, name the test in the specification, agree the acceptance criteria with the supplier, and ask whether results exist for the exact pretreatment and coating system being bought.
Preventing filiform corrosion
In the specification
- Pretreatment: ask the coater to state it and to support it with evidence for the exposure.
- Primer and topcoat: specify a matched system chosen for the environment, not a topcoat alone.
- Test evidence: where it matters, name EN ISO 4623-2 and agree the acceptance criteria.
- Edge treatment: if parts will have exposed cut edges in a humid or coastal setting, state how edges are to be treated.
Orbit supplies coil-coated aluminum on 3105 and other 1xxx, 3xxx and 5xxx substrates in PE, HDPE, PVDF, PU, PUPA, Epoxy, Acrylic and Epoxy-PE systems. State the exposure and any test requirement in the RFQ.
In fabrication and handling
- Protect cut edges. Detail edges so they drain and stay out of standing water, and seal or touch up edges where the specification calls for it, with a product compatible with the coating.
- Avoid coating damage. Keep tooling clean, do not drag sheets across each other, and keep protective film in place through handling, and remove it within the film supplier's stated exposure limit.
- Repair scratches promptly. Use a touch-up product compatible with the coating system. A scratch left open is a starting point.
- Keep coil and sheet dry. Store indoors, off the floor and away from condensation, and inspect packaging on arrival. The guide to receiving, storing and handling coated coil sets out the checks.
Standards referenced
- EN ISO 4623-2, Paints and varnishes. Determination of resistance to filiform corrosion. Part 2: Aluminium substrates
Filiform questions.
What causes filiform corrosion?
It starts at a break in the coating, such as a cut edge, scratch or defect, where moisture and a contaminant such as chloride reach the metal. It then spreads as threads along the boundary between the metal and the coating.
Why does filiform corrosion start at cut edges?
A cut edge exposes bare metal and the boundary between metal, pretreatment and paint, with no coating over it. Moisture and salts can reach that boundary directly.
How is filiform corrosion tested on coated aluminum?
EN ISO 4623-2 covers coated aluminum. Coated panels are scribed through the coating, exposed to conditions that promote filiform corrosion, and examined for thread-like corrosion spreading from the scribe.
Does a thicker coating prevent filiform corrosion?
Pretreatment and coating system both matter; ask for filiform test data (EN ISO 4623-2).
How should cut edges be protected?
Detail edges so they drain and stay dry, keep them out of standing water, and seal or touch up edges where the specification calls for it, using a product compatible with the coating.
Can scratches in the coating be repaired?
Yes. Repair them promptly with a touch-up product compatible with the coating system, because an open scratch is a possible starting point for filiform corrosion.
Coated coil for a humid or coastal site?
Send the alloy, coating system, exposure, any test requirement, thickness, width, quantity and destination. We respond to RFQs within one business day.