Reference · Coating tests
Coated aluminum test methods: what each test measures.
Coated aluminum test methods are standardized laboratory checks that show whether the paint film on coil has the thickness, cure, hardness, adhesion, flexibility and appearance a specification asks for. Each test measures one property under defined conditions, and none of them on its own predicts years of service outdoors. Below: what each test measures, what it leaves out, and links to the detailed guides.
- Standardized laboratory methods
- ASTM or EN, depending on market
- Reports per system and color on request
Coated aluminum test methods with a full guide.
Four tests have their own reference page covering the method, the panel preparation and how to read the result.
Salt spray
Accelerated corrosion exposure in a salt fog cabinet run to ASTM B117. Useful for ranking systems and lots tested the same way; the hours do not convert into years.
Salt spray test (ASTM B117)Color difference
A single number for how far a measured color sits from the approved standard. It needs the formula, the instrument conditions and the reference stated with it.
Delta E for coated coilPencil hardness
Graded pencils pushed across the cured film show how well the surface resists scratching and gouging. Quick to run, but sensitive to the operator and the pencils.
How the pencil hardness test worksCross hatch adhesion
Cuts through the film, tape pressed on and pulled off, removal rated against a scale. The measured film thickness decides whether an X-cut or a lattice is used.
Cross hatch adhesion test guideWhat do the other coating tests measure?
The tests below appear on datasheets and test reports for coated coil but do not have a page of their own here. Pass levels come from the specification, so none are given.
T-bend flexibility (ASTM D4145, EN 13523-7)
ASTM D4145 is titled "Coating Flexibility of Prepainted Sheet", and EN 13523-7 is the T-bend part of the EN coil coating test series. A strip of coated sheet is bent back on itself with the paint outside, then bent again around the folded part, each fold widening the inside of the bend by one sheet thickness. The bend is checked for cracking and, with tape, for loss of adhesion. The result is a T value: the number of sheet thicknesses inside the tightest bend that passes.
It does not tell you how the film behaves on a specific roll-formed profile or at a temperature other than the test temperature. Alloy, temper and thickness change how the metal bends, so T values are compared only on the same substrate.
Solvent rub resistance (MEK rub)
A cloth soaked in a solvent such as methyl ethyl ketone (MEK) is rubbed back and forth over the film, counting double rubs, until the film wears through or an agreed count is reached. ASTM D5402 describes a solvent rub practice for cured organic coatings, and the EN 13523 series has a part for solvent resistance; the solvent and rub count are agreed between the parties. It is mainly a check on cure: an undercured film softens and wears through sooner.
It does not measure resistance to the chemicals a panel meets in service, such as cleaners or pollutants, and counts from different resin chemistries are not directly comparable.
UV weathering in fluorescent UV cabinets (ASTM G154)
ASTM G154 is titled "Operating Fluorescent Ultraviolet (UV) Lamp Apparatus for Exposure of Materials". Panels are exposed to ultraviolet light from fluorescent lamps, typically in cycles with periods of moisture, then checked for loss of gloss, color change and chalking. Like the salt spray practice, it defines how the apparatus is run; the cycle, the duration and the acceptance limits come from the specification.
Fluorescent UV lamps do not reproduce the full spectrum of sunlight, and the cabinet leaves out a real site's dirt, pollution and temperature range. Results rank coatings run in the same cycle; they do not convert into years outdoors, and some coatings rank differently outdoors.
Impact resistance (ASTM D2794)
ASTM D2794 covers "Resistance of Organic Coatings to the Effects of Rapid Deformation (Impact)". A weight is dropped from increasing heights onto an indenter resting on the panel, striking either the coated face or the reverse side, and the deformed area is examined for cracking. The result is the highest impact the film withstands without failing.
It does not measure the dent resistance of the panel, which depends on metal thickness and temper, or the hail performance of a finished roof. Results are compared on the same substrate.
Specular gloss (ASTM D523, EN 13523-2)
ASTM D523 is titled "Specular Gloss", and EN 13523-2 is the coil coating method for it. A glossmeter shines light onto the surface at a defined angle and measures how much is reflected at the mirror angle, relative to a reference standard. The reading is given in gloss units at the angle used, chosen to suit the gloss level of the finish.
A gloss value says nothing about color or durability. Readings at different angles cannot be compared, and textured, wood grain or metallic finishes are usually also checked against an approved sample. Gloss retention needs readings before and after exposure, taken the same way.
Dry film thickness (ASTM D7091, EN 13523-1)
Film thickness is measured with a nondestructive gauge on the cured panel. ASTM D7091 covers nondestructive dry film thickness measurement on metal substrates, and EN 13523-1 is the coil coating method for film thickness. Aluminum is not magnetic, so gauges for it work on the eddy current principle.
The gauge reads the total film above the metal, primer and topcoat together. Thickness is a precondition, not proof of performance: a film at the right thickness can still be undercured or poorly bonded.
How to read a coating test report
A test result means something only against three things the report should state.
- Same method. ASTM and EN methods for the same property can differ in details such as apparatus, panel size and rating scale, so a figure from one is not compared directly with a figure from the other.
- Same panel preparation. Alloy, temper, thickness, pretreatment, film thickness, cure and conditioning all change results. Panels cut from production or trial coil carry the real pretreatment and paint system.
- Agreed acceptance criteria. A method says how to test; the pass level comes from the coating specification or the purchase agreement.
Orbit works to ASTM or EN depending on the market and supplies material certificates with every batch. Coating test reports for a given system and color on prepainted aluminum coil are available on request; name the system, the color and the tests you need with your RFQ. If the system is not chosen yet, start with the coating systems Orbit applies.
Coating test questions.
Which tests are used on coated aluminum coil?
Tests used on coated coil include film thickness, gloss, color difference, pencil hardness, adhesion, T-bend flexibility, impact, solvent rub, salt spray and UV weathering. Which ones apply, and the pass levels, are set by the coating specification.
Do these tests predict how long a coating will last?
No. Each test measures one property under laboratory conditions. Accelerated exposures such as salt spray and fluorescent UV rank coatings tested the same way, but their hours do not convert into years outdoors.
Should a coating be tested to ASTM or EN methods?
It depends on the market and on the specification that applies. Orbit works to ASTM or EN depending on the market. Compare results only when they come from the same method.
What does a T-bend value mean?
It is the number of sheet thicknesses inside the tightest bend at which the film passes the agreed check for cracking and loss of adhesion. A lower value means the film survived a tighter bend on that substrate.
Why does film thickness matter for other tests?
Thickness affects how a film performs in most other tests, and it decides which tape adhesion method applies. A report should state the measured film thickness of the panels tested.
Can Orbit provide coating test reports?
Yes. Test reports for a given coating system and color are available on request; state both, and the tests you need, with your RFQ.
Need test reports for a coating system?