Reference · Temper

Aluminum temper chart: F, O, H, W and T designations.

This aluminum temper chart explains what the letters and digits after an alloy number mean. The letter gives the basic condition. For the alloys on this page the letters you will see are F (as fabricated), O (annealed) and H (strain hardened); T (thermally treated) applies to heat-treatable alloys. ANSI H35.1 and EN 515 also define W, an unstable temper after solution heat treatment that applies to heat-treatable alloys only. For H tempers, the first digit gives the treatment after strain hardening and the second digit gives how hard the metal is, from quarter hard to extra hard.

  • Basic tempers F, O, H, W, T
  • H1x to H4x
  • Second digit 1 to 9
  • ANSI H35.1 and EN 515

How to read an aluminum temper chart

An aluminum alloy number describes the chemistry. The temper designation describes the condition that chemistry was left in by rolling and any heat treatment. The two are written together, alloy first, then a hyphen, then the temper: in 5052-H32, for example, 5052 is the alloy and H32 the temper. (The example shows the notation only.)

The temper starts with one of the basic letters below. Some tempers stop at the letter. Others add digits that narrow the condition down.

Basic aluminum temper designations
LetterNameWhat it means
FAs fabricatedProduct left in the condition the forming process produced, with no special control over strain hardening or heat treatment.
OAnnealedHeated to bring the metal to its softest, most formable condition.
HStrain hardenedStrength raised by cold work, such as cold rolling. Always followed by digits.
WSolution heat treatedAn unstable temper after solution heat treatment. Applies to heat-treatable alloys only.
TThermally treatedThermally treated to produce stable tempers other than F, O or H. Always followed by digits.

H tempers apply to alloys that gain strength through cold work. T tempers apply to heat-treatable alloys. Orbit rolls 1xxx, 3xxx and 5xxx series alloys, which are strengthened by cold work rather than by heat treatment, so T tempers do not apply to them.

H temper designations: the first digit

After the H, the first digit says what was done to the metal after it was strain hardened.

First digit after H: treatment after strain hardening
DesignationMeaning
H1xStrain hardened only. The strength comes from cold work alone, with no heat treatment afterward.
H2xStrain hardened, then partially annealed: heat brings part of the hardness from cold work back down.
H3xStrain hardened and stabilized. The designation standards set out when stabilization applies. Stabilization applies to magnesium-containing alloys, such as 5xxx, that would otherwise soften slowly at room temperature.
H4xStrain hardened, then lacquered or painted: the metal is heated during the paint cure.

H4x is the one group defined by a coating step. It matters to buyers of painted coil because the paint cure is a heat treatment of its own, and it can move the properties of the substrate.

Second digit: how hard the temper is

The second digit after the H gives the degree of strain hardening that remains in the metal. The even digits mark fixed points on the scale; the odd digits fall between them.

Second digit after H: degree of strain hardening
Second digitDegree of hardnessExample form
2Quarter hardH12, H22, H32
4Half hardH14, H24, H34
6Three-quarter hardH16, H26, H36
8Full hardH18, H28, H38
9Extra hardH19, H29, H39
1, 3, 5, 7Intermediate, between the even digits on either sideH13 sits between H12 and H14

Read the two digits together. H14 and H24 are both half hard, but H14 reached that point by cold work alone, while H24 reached it by strain hardening followed by partial annealing. They are different tempers, which is why the first digit belongs on the order as well as the second. The example forms show how the codes are built; they are not a list of tempers made in any alloy.

As a general rule, a higher second digit means more strength and less formability. The values that go with each code are set per alloy and product in the product standard, not by the designation.

Some tempers carry an optional third digit, which marks a variation of the two-digit temper and is defined in the designation standards rather than here.

What T tempers mean

A T temper means the metal has been thermally treated to produce a stable temper other than F, O or H. The T is always followed by one or more digits that identify the treatment sequence. T tempers belong to heat-treatable alloys, which get their strength mainly from heat treatment rather than from cold work.

This chart does not list the individual T codes, because they do not apply to the 1xxx, 3xxx and 5xxx alloys Orbit rolls. For a heat-treatable alloy, read the T designations in ANSI H35.1 or EN 515 together with the product standard for that alloy.

Which standards define aluminum tempers?

Two designation standards set out the system:

  • ANSI H35.1 covers alloy and temper designations for aluminum in US practice.
  • EN 515 covers temper designations for wrought aluminum products in European practice.

These standards define what a code means. They do not say which tempers a mill offers in a given alloy, or what strength each temper must reach. That is the job of the product standard: ASTM B209 for aluminum sheet and plate in US practice, and EN 485-2 for mechanical properties in European practice.

Which tempers are available in each alloy?

The tempers available depend on the alloy and the product. The product standard lists the alloy and temper combinations it covers, with the mechanical property limits for each, so check ASTM B209 or EN 485-2 for the combination you need rather than a general chart. A temper that appears in a standard is not automatically one that every mill rolls in every thickness.

Orbit confirms the alloy and temper per order. When you send an RFQ, state:

  • The alloy and the full temper designation, including both digits after the H.
  • The product standard the material is to meet, ASTM or EN depending on your market.
  • The thickness, width and finish, because the temper you can get may depend on them.
  • The forming step, if the part is bent, roll formed or deep drawn after delivery.

Every batch ships with material certificates that record the alloy and temper supplied. For coil that is coated and then formed, the guide on choosing temper for coil coating and forming covers how to weigh bend radius against dent resistance. Orbit quotes rolled aluminum coil from 0.20 to 2.00 mm thick and up to 1650 mm wide, and replies to an RFQ within one business day.

Aluminum temper questions.

What does the H mean in an aluminum temper?

H means strain hardened: the metal has gained strength through cold work such as cold rolling. It is always followed by digits. The first digit gives the treatment after strain hardening and the second the degree of hardness.

What is the difference between H14 and H24?

Both are half hard. H14 is strain hardened only, while H24 is strain hardened and then partially annealed to reach half hard. They are different tempers with their own property limits in the product standard, so state the full designation on the order.

What does O temper mean?

O means annealed: the metal has been heated to its softest and most formable condition. It has the lowest strength of the tempers for a given alloy.

Is a higher second digit always harder?

Within one first-digit group of the same alloy, a higher second digit means a greater degree of strain hardening: 2 is quarter hard, 4 half hard, 6 three-quarter hard, 8 full hard and 9 extra hard, with odd digits in between. The property values for each code are set in the product standard.

Which standard defines aluminum temper designations?

ANSI H35.1 in US practice and EN 515 in European practice. Product standards such as ASTM B209 and EN 485-2 then list the tempers they cover and the mechanical properties each must meet.

Which tempers can Orbit supply?

Orbit rolls 1xxx, 3xxx and 5xxx series alloys. The tempers available depend on the alloy and product, and the alloy and temper are confirmed per order against the ASTM or EN product standard for your market.

Have an alloy and temper to quote?

Send the alloy, full temper designation, product standard, thickness, width, finish, quantity and destination. We respond to RFQs within one business day.

Request a Quote