Seven Coil Alloys in One Table: What It Shows and What It Leaves Out.
One table can orient a reader quickly. It can also tempt a reader to pick an alloy from it. This post gives the table and then spends as long on what the table cannot decide.
Key takeaways
- The table groups the alloys by series, main alloying element and strengthening route. It carries no property values.
- All seven alloys are non-heat-treatable. Cold work, recorded in the temper, raises strength together with alloying content.
- Choosing needs more than a table: forming, strength in your temper, exposure and coating.
- Use the Teal Sheets for composition limits, the standard's tables for requirements and the certificate for the lot.
What does the table show?
| Alloy | Series | Main alloying element | Heat treatable? | Read next |
|---|---|---|---|---|
| 1050 | 1xxx | None; commercially pure aluminum | No | 1xxx guide |
| 1100 | 1xxx | None; commercially pure aluminum | No | 1xxx guide |
| 3003 | 3xxx | Manganese | No | 3xxx guide |
| 3105 | 3xxx | Manganese | No | 3xxx guide |
| 5005 | 5xxx | Magnesium | No | 5xxx guide |
| 5052 | 5xxx | Magnesium | No | 5xxx guide |
| 5754 | 5xxx | Magnesium | No | 5xxx guide |
The first digit of the designation identifies the alloy series, which for 2xxx through 7xxx corresponds to the main alloying element, for 1xxx is commercially pure aluminum and for 8xxx covers other elements, and the Aluminum Association registers each designation and its composition limits in the Teal Sheets.
Why are all of them non-heat-treatable?
The table lists none of the alloys as heat treatable because strength in these alloys is raised by cold work such as cold rolling, together with alloying content, not by a heat treatment cycle. The H temper designations record how the strain hardening was done. So for these alloys a request that names the alloy but not the temper leaves out a major part of what sets strength and formability.
What can the table not decide?
- Strength in your temper: read it from the tables of the standard on your order, such as ASTM B209/B209M, not from the series number.
- Formability for your bend: depends on temper, gauge and the forming method.
- Exposure: alloy is one input next to the coating, pretreatment, edges and maintenance.
- The lot you receive: the material certificate that ships with each batch reports what was tested.
How do you get from the table to a short list?
- Filter the seven alloys by the temper and mechanical properties your specification names, using the requirement tables of the standard on your order.
- Filter what remains by forming severity: bend radius against thickness, forming method and part geometry.
- Filter again by exposure and finish.
Send the short list to the supplier with your specification and ask for a written reply that proposes alloy and temper against it. The reply, not the table, chooses among the candidates.
Where do the standards fit?
Composition limits come from the Teal Sheets or the composition standard named on your order. Requirement tables come from the product standard, ASTM or EN depending on your market. Reported values for your lot come from the certificate. The datasheet reading guide shows how to compare a requirement with a typical value, and the temper guide explains the designations.
What to send with a request
If the alloy is open, send the part description rather than guessing: forming operation, gauge range, width, exposure, coating and finish, and the quantity. If the alloy is fixed, send alloy and temper with the standard. Either way Orbit replies within one business day with what it can confirm. Orbit also rolls coil from 0.20 to 2.00 mm thick and up to 1650 mm wide, so check your gauge and width against that range. For a head-to-head on two of the rows, see 3003 vs 5052 for outdoor coil coating.
What does the table say about 1xxx and the others side by side?
It says only how they are classified. The 1xxx rows carry no main alloying element, because those alloys are commercially pure aluminum, and the 3xxx and 5xxx rows name manganese and magnesium. That difference in composition is why the designation system places them in separate series, and it is the starting point for reading each family guide. It does not rank the alloys, and the table gives no basis for saying that one row suits a part better than another.
How should a buyer use the table with a drawing?
Mark the drawing with the forming operations and the gauge. Write the strength the part needs in service. Then add the exposure and the finish. With those four items in hand, the table gives the candidate families and the family guides give the questions to ask about each. The supplier should then confirm an alloy and temper in writing, with the standard they apply, and that confirmation is what goes on the purchase order.
Keep the table with the request, not with the decision. If the drawing changes, the candidates change with it, and the table is quick to re-read.
How can the table be misread?
- Reading a higher series number as a better alloy. The first digit identifies the alloy family, not a grade.
- Reading "not heat treatable" as "not strengthenable". Cold work strengthens these alloys, and the temper records it.
- Reading a row as a specification. A row names an alloy. A specification adds the temper, thickness, width, tolerance standard and coating.
Common questions
Which alloy on the list should I choose?
That depends on the use. The choice depends on forming, strength in the temper, exposure and coating.
Why does the table not list strength values?
Strength depends on temper and thickness. Values belong to the standard's tables and to your certificate, not to a series summary.
Are any of the alloys heat treatable?
Not the ones on this list. Their strength comes from alloying content and cold work. The temper records the cold work.
References
- The Aluminum Association: International Alloy Designations and Chemical Composition Limits for Wrought Aluminum and Wrought Aluminum Alloys (Teal Sheets): the registry of designations and composition limits.
- ASTM International: B209/B209M, Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate: the requirement tables for sheet, coiled sheet and plate.
Not sure which alloy?